2021年2月12日发(作者:结案陈词)


1


.你现在有空吗,我可以问你一些问题吗?



Could I ask you some questions if you are free?/ Are you free now? May I ask you


some questions (a question)?


2




请问此 产品的面是否为外观面?表面做什么处理?是晒纹


/


抛光?



Can you tell me whether the surface of this part is a visible/esthetic one? What


will we do for its surface? Texture or Polishing?


3




请问产品这个面可否加顶针或顶块?产品允许加扁顶针吗?



Does this part need an ejector pin or an ejector bar? Can we add an ejector blade?


4




这个产品的柱位我们打算做司筒。(或镶针)可以吗?



Can we add ejector sleeves or ejector pins in the boss of this part?


5




产品的 这个位置不能出模,我们打算做行位,在此面上会有分模线,你接受吗?



There''s an undercut at this position and it needs a slider. It will also have a


parting line on this side, is that OK?


6




产品里面的这个位置我们打算做斜顶或内行位,有问题吗?



We


will


make


the


lifter


and


(inner)


slider


in


this


position,


will


that


be


a


problem?


7




你提供 的


2D


产品图与


3D

< br>产品图不一致,请问以哪一个图面为准?



The 2D and 3D drawing you provided is not the same, can you tell me which one is


correct?


8




你提供 的


3D


产品图有的地方没有出模角,有的地方胶位太厚,有的地 方胶位太溥,这


些产品问题我们可以自己修改吗?修改后会给交给你确认。



There is no draft angle in the 3D drawing, some materials are too thick, and some


place are too thin. Can we modify this part by ourselves? We will send the drawing


to you for you to check after we modify it.


9




按你们提供的缩水率千分之五,


这个模具的尺寸已经做到了模具图面要求。

< p>
但注塑出来


的产品不符合你们的产品图。请确认你们的材料的缩水率是否正 确?



According


to


the


shrinkage


one


over


two


hundred,


the


mold


has


been


done


in


the


right


dimension,


but


the


part


falls


short


to


your


part


drawing,


are


you


sure


the


shrinkage


is right?


10




产品 的这个位置太小,导致模具钢料太溥,能够加宽这个位置吗?



This position is too small and will make the steel material here too thin, can we


widen it here?


11




斜顶 与后面的柱位空间太小,


斜顶在运动时会干涉到柱子,


能移动这 个柱子的位置吗?



The angular lifter interferes with the boss during ejection. Please consider


changing the position of the boss.


12




这个筋骨位胶厚太薄,而且高度偏高,注塑时很难填充这个筋位,可以增加这个筋骨

位的厚度吗?



The rib here is too thin and on the high side, so it will be difficult to fill here


when we do the injection, can you increase the thickness of this rib?


13




你是 想将此筋骨位的高度加高


/


减低吗?加胶的位置我们将用铜公放 电加深。


但减胶的


位置有两种做法,


1


、做镶件;


2


、烧焊;因为镶件的底部 有运水,我们简单的做法是烧焊处


理,你可以接受吗?



Will you increase/decrease the material on this rib? We will use EDM if you add


material, but there are two options if you choose to decrease: inserts;


g, because there is water in the bottom of the insert, is that OK?


14




这个 样板的筋骨位底部烧焦,是因为排气不良,我们可以在筋骨位的中间增加一个镶


件。



This sample has been burned in the bottom because the venting is not good, we can


add an insert in the middle of the rib.


15



< br>重做镶件大约需要


5-6


天时间,你能接受吗?



It will take about 5 or 6 days to redo the insert, is that OK?


16




产品 的这个面我们已经做了晒纹处理,


如果需要加胶,


这个面我们需 要重新外发晒纹。


可能需要几天的时间。所以我们直接以铜公放电的火花纹取代你要求的 纹路,你可以接受


吗?



We have made the texture on this side, if we add material, it will take some days


to remake the texture by out-resourcing, so we suggest using the texture by EDM


instead, is that OK?


17




模具 是用公制


/


英制的配件?需要备用件吗?



Is this mold dimension measured in inches or meters? Does it need spare parts?


18




模具 上铭牌上的刻字内容是由你们提供吗?你们什么时候可以这些刻字资料。



Will you provide the engraving content of the plate of this mold to us? When will


you send it?


19




可否 提供此模具生产时,注塑机的型号及相关资料。如:啤机大小、呵林柱尺寸、顶


棍孔尺寸 等



Can


you


provide


the


type


of


injection


machine


and


other


related


information


of


this


mold to us? Such as the boss dimension, the hole''s dimension of the ejector pin


and the size of the injection machine and so on.


20




这个问题我需要同其它同事商议会再答复你。



I


need


to


discuss


this


problem


with


the


other


colleagues


and


then


I


will


reply


back


to you.


21




我们将尽力达成你的计划,如有异常,会及时通知你。



We


will


try


our


best


to


complete


your


plan,


if


there


are


any


complications,


we


will


notify you immediately.


22.


这个产品的长度为


330.12 MM,


宽度为


78.96MM,


高度为


45MM.


胶厚为


2MM,

< p>
重量为


70.63g,


试模注塑机型号为


250



,


胶料颜色为 黑色


,


产品外表面晒纹处理


,


内表面为抛光


.


需要日期


章、环保章、材料章


.


前后模用


23 44


氮硬,斜顶和行位座用


738H


, 以上模具信息正确吗?


请确认!




is 2MM,


weight is


70.63g, the injection machine


is 250T,the


material


is


black,


the


outside of the part has texture, inner side needs polishing, and it also needs a


date and recycle stamp, the core & cavity is 2344 nitridng, the lifter and slider


shelf is 728H. Please check the information above!


23




现在到了吃午饭的时间,我们下午再继续好吗?



It is time to have lunch, let''s discuss this project later this afternoon?


24.


和滑块干涉的倒勾请加料填平至滑块可以顺利滑动



(The undercut area interferes with the slide block and needs to be filled with


material to help the slider move smoothly.)


25.


加肉太多


(The thickness added is too thick.)


26.


加肉面积太大


(The thickening area is too wide.)



位置移位


( The gate position is moved.)


28.


滑块拆的位置


(The split line of slide block or the area of slide.)


29.


此处有尖角,填充困难


(It is hard to fill this area due to the sharp feature.)


30.


此处钢材太薄,强度不足而且不容易冷却



(The strength of this area is too weak and it is hard to cool because the steel is


too thin.)


31.


圆柱 特征要有一半圆不可以拆在滑块上,以免粘滑块造成拉白,拉断



(We avoid designing the semicircle of the cylinder on the slide block because it


will be pulled apart or cause drag marks.)


32.


此处做斜销在作动时会削到成品肉厚



(The part will be damaged if we make the lifter in this area.)


33.


这个面是装配面,不能加料



(This is a critical surface where we cannot add additional material.)


34.


此处料位太厚,会有缩水,建议减料改善



(Because


of


the


shrinkage


of


the


thickness,


we


suggest


reducing


some


wall


thickness


to improve it.)


35.


此面是不是外观面,此处做滑块的话会有夹线,是否可以接受




critical


surface or not. Also, confirm whether it


is acceptable to have a slide split line if we have a slide in this area. )


36.


此处有倒勾,能否减料,使公母模靠破,不做滑块和斜销




confirm


whether


we


can


reduce


material


to


the


area


where


we


have


an


undercut


as indicated to have shut off on cavity side. No slide block and lifter will be


made. )


37.


请尽快确认这种拆模方式和结构,否则会影响模期



(Please


confirm


the


issues


of


Parting


line,


Gate


position...Etc.


as


soon


as


possible;


otherwise, the lead-time will be extended.)


38.


此面是否有特殊要求,能否有顶针印



(Please


confirm


whether


it


is


a


critical


surface


or


not


and


if


we


can


have


E.J.


pin


marks on it.)


39. P.L


面开在此处,模具上会有尖角和刀口,对模具寿命有影响



(There


are


sharp


edges


if


we


set


the


parting


line


here,


It


will


reduce


the


tool


life)


40.


加大拔模角,以便脱模顺利



(We suggest enlarging the draft angle to help release the tool.)


41. GATE


做在此处的话有两个 缺点:


1.


盖子打开时可以看到


GAT E


的修剪部位


; 2.


两个斜销


在同一侧,顶出也不是很平衡


.


(There are two problems if the gate is to be designed in this area:


a). It is easy to see the gate mark when you open the cap.


b). The ejectors are unbalanced when two lifters are on the same side)


42. GATE


做在此处的话


.


盖子打开后看 不到


GATE


的修剪部位



(The gate mark is not visible if the gate position is designed like this.)


43.


如果


GATE


一定要做在你们指定的位置的话,那还不如做在这一侧,这样的话还可以减


小这 个位置的缩水




would further recommend to have


it to the area indicated so it can avoid a shrink problem in this area.)


44.


在此处


GATE


做潜顶针的话,背后的外观面会有冲料痕,而且成品又是黑色的,会最明




(If the design of the gate has to be a sub. Gate, then the back surface of the part


will have serious flow marks due to the black colour.)


22. P.L


开在此处不合理,模具加工困难,


P.L


应改为和图示的一样




area


is


not


suitable


to


have


a


Parting


line


because


the


tool


will


become


more


complicated; therefore, we recommend to have the Parting line as indicated .)


45


。产品粘母模的机会很大,能否在公模加倒勾,


拉料顶针或者公模保留


E.D.M


纹,开模时


使成品留在公模一侧




make undercuts, snatch pins or leave coarse E.D.M. on the core to snatch the part


on)


46.


此处料厚段 差很大,成品表面会有应力痕,是否接受



(Please


confirm


whether


it


is


acceptable


to


have


stress


lines


on


the


surface


because


the thickness is not equal.)


47.


请注明何处为外观面,能否提供


2D


图和注意事项



(Please advise where the critical surface is. Please also provide us a 2D drawing


with critical dimensions. )


48.


红色所示处是有问题的地方,请特别注意



(Please note the red highlights because those areas have problems.)


49.


成品设计此处有问题,建议如下图所示修改



(We


would


suggest


using


the


attached


part


design


as


the


current


design


has


problems.)


50.


此处改为一个球形的凹槽


(We suggest modifying it as a globe recess.)


51.


圆柱特征要有一半不可以拆在滑块里,以防拉断


(this issue is the same as no.8)


52.


此处大滑块上走小滑块,小滑块要先退,大滑块要做延迟



(The inside small slide block will recede first and the parent slide block have to


postpone sliding.)


53.


滑块要用液压油缸抽芯以保证开合模顺序



(The slide pins will use an oil cylinder to assure that the process is in proper


order.)


54.


这个面有装配,加料的话装配时会顶住,如图所示




add material to this


surface because it will


intervene between the two


parts when it is assembled. Please see the sketch attached. )


55.


可降低斜销面,增加成品些许肉厚来做变化



(To descend the surface of lifter in order to thicken the part.)


56.


一半做斜销,一半做自然


(One half side will have the lifter and the other half


will be solid/nature.)


57.


此处两个柱子重迭,有倒勾,不能做自然,要做


SLIDE



solid. We suggest making it with a slide block.)


58.


此处强迫顶出


(This area needs force ejection.)


59.


公模两段开模,这个地方先退


(Here will be a double ejection for forward and


receding.)


60.


此处做镶件会有夹线,能否接受



(Please confirm whether it is acceptable that there will be a split line here.)


61.


此面公母模


1


度靠破,会有段差,可否接受



(Please


confirm


whether


it


is


ok


to


have


mismatch


to


the


area


where


there


is


1


degree


of shut off in Core / Cavity side.)


62.


这个尺寸能否加大


(Please confirm whether we can enlarge this dimension.)


63.


此处加一个凹槽,胶片的弹出效果会更好一些,试模后 看装配的效果再做修正




will affect


the


elastic


of the film


better


if we add a recess. See


how it will


affect the assembly parts, and then make your decision.)


64.


此处有倒勾,建议将剖面线所示部位


CUT


即可避免此处的倒 勾



(There is an undercut here, we suggest cutting out the indicated part as it


highlighted to avoid an undercut.)


65.


成型后


SUB


GATE


要修平


(The


gate


(sub


gate)


needs


to


be


trimmed


evenly


after


being


moulded.)


66.


此处倒勾先垂直顶出,之后再手动取出



(This


area


of


the


undercut


needs


to


be


ejected


vertically,


then


taken


out


manually.)


67.


这两 个面都有滑块,


GATE


改在此处改不到



(The


gate


is


not


suitable


in


this


area


becuase


there


are


two


sliding


blocks


sealing


off this area.)


68.


此处加做一个旋转


GATE< /p>


,射出时方便调整成品的质量


-


-


-


-


-


-


-


-



本文更新与2021-02-12 21:00,由作者提供,不代表本网站立场,转载请注明出处:https://www.bjmy2z.cn/gaokao/645768.html

试模问题点常用英文的相关文章